Table 1 Textural properties of the catalysts from N 2 adsorption measurements

From: Influence of crystal structure of nanosized ZrO2 on photocatalytic degradation of methyl orange

Catalyst

S BET (m 2 g −1 )

V p (cm 3 g −1 )

Pore radius (Å)

m-ZrO2

65

0.626

50.0

t-ZrO2

74

0.521

28.3

c-ZrO2

204

0.508

19.0