Figure 4From: Investigation on the passivated Si/Al2O3 interface fabricated by non-vacuum spatial atomic layer deposition system Optical microscope images for different thicknesses of Al 2 O 3 film annealed at 500°C. (a) 10 nm, (b) 15 nm, (c) 20 nm, (d) 25 nm.Back to article page