Figure 6

Assembly courses dependent on the electric field strength ( E ) in a suspension of DNA-CNT mixture ( α=1 ). (a) The normalized mean darkness G(t) of the CNT assembly area is plotted as a function of the duration time, t, to compare the time courses for E=25 kV/m (blue squares), E=50 kV/m (red circles), E=100 kV/m (green crosses), and E=200 kV/m (orange triangles) at the same frequency of f=20 MHz. (b) Log-log plot of the inverse required times, 1/t req, versus E at f=20 MHz. A light blue line, representing the proportionality of 1/t req to E 2, is shown for comparison. Standard errors fall within symbols.