Table 3 The comparison of the properties between the CoFe 2 O 4 /SrFe 12 O 19 nanocomposites prepared by electrospinning and other methods

From: A novel method to fabricate CoFe2O4/SrFe12O19 composite ferrite nanofibers with enhanced exchange coupling effect

Preparation method

M s (emu/g)

H c (Oe)

Structure

Annealing temperature

Reference

Coprecipitation

27.9

3,567

Core-shell nanoparticle

800°C

[15]

Modified flux method

50

1,798

Nanoparticle

900°C

[14]

Coprecipitation

42.5

2,475

Nanoparticle

1,000°C

[16]

Electrospinning

60.9

3,190

Nanofibers

900°C

Our group [9]

Electrospinning

62.8

2,290

Nanofibers

800°C

This work