Figure 16
From: Obtaining of Ni/NiO nanopowder from aqua solutions of Ni(CH3COO)2 ammonia complexes

Powders’ free carbon content and specific surface area at various ammonia content in complex (350°C, 60 min).
From: Obtaining of Ni/NiO nanopowder from aqua solutions of Ni(CH3COO)2 ammonia complexes
Powders’ free carbon content and specific surface area at various ammonia content in complex (350°C, 60 min).