Fig. 6 | Nanoscale Research Letters

Fig. 6

From: Conductivity of PEDOT:PSS on Spin-Coated and Drop Cast Nanofibrillar Cellulose Thin Films

Fig. 6

Left hand column, annealed (130 °C) and freeze fractured samples: (a) PEDOT:PSS reference, thickness 47 nm; (b1) PEDOT:PSS on spin-coated NFC-G, thickness 138–145 nm; (c1) PEDOT:PSS on drop cast NFC-G, thickness 438–458 nm. Right hand column samples without annealing and freeze fracturing: (b2) PEDOT:PSS on spin-coated NFC-G, thickness 127 nm; (c2) PEDOT:PSS on drop cast NFC-G, thickness 274 nm