Fig. 8From: Structure and Strength of Iron-Copper-Carbon Nanotube NanocompositesThermopower of Fe-Cu (4:1) precursor specimens rolled with relative deformation of ε Σ = 70 (1, 3, 5) and 95 (2, 4, 6) % treated in the planetary mill during 20 (1, 2), 60 (3, 4) and 120 (5, 6) minutes against the time of step-by-step annealing at the temperature values given on the figureBack to article page