Skip to main content

Advertisement

Table 5 Thickness, electrical conductance, and electrical conductivity of the HCNFs and CNFs

From: Control of physical properties of carbon nanofibers obtained from coaxial electrospinning of PMMA and PAN with adjustable inner/outer nozzle-ends

Sample Thickness (μm) Conductance (S) Conductivity (S m−1)
Inward coaxial nozzle 10.82 626.00 376
Normal coaxial nozzle 13.22 882.54 648
Outward coaxial nozzle 5.58 2176.58 675
Single nozzle 10.72 1850.63 1102