Fig. 6From: Influence of the Shell Thickness and Ratio Between Core Elements on Photostability of the CdTe/CdS Core/Shell Quantum Dots Embedded in a Polymer Matrix a Irradiation time dependence of photoluminescence energy maximum of the polymer composites containing CdTe/CdS quantum dots with different passivation times: 1–0.5, 2–2, 3–6, 4–16, and 5–26 h. b Dependence of the Pl energy maximum shift rate on the passivation time of quantum dotsBack to article page