Fig. 4From: Electrical Characterization of Amorphous Silicon MIS-Based Structures for HIT Solar Cell ApplicationsInterfacial state densities measured by DLTS corresponding to all deposition temperatures. D it profile obtained for a sample grown at 30 °C without previous RCA treatment is also shown for comparisonBack to article page