Fig. 4From: Oxidation Resistance of Materials Based on Ti3AlC2 Nanolaminate at 600 °C in AirBack-scattered electron images of the scales formed at 600 °C for 1000 h: a Ti3AlC2-based material with 22 % porosity, b oxidized pores of Ti3AlC2-based material with 22 % porosity, d Ti3AlC2-based material with 1 % porosity, e Nb alloyed Ti3AlC2-based material with 1 % porosity, and c scale surface of Ti3AlC2-based material with 1 % porosity after 15 h oxidationBack to article page