Table 2 Parameters of CuO-Cu2O complex thin film-based perovskite solar cells following thermal oxidation of the film at various temperatures
From: Nano-structured CuO-Cu2O Complex Thin Film for Application in CH3NH3PbI3 Perovskite Solar Cells
Annealing temp. (°C) | VOC(V) | JSC(mA/cm2) | FF(%) | Eff(%) | Rs(Ω) | Rsh(Ω) |
---|---|---|---|---|---|---|
300 | 0.88 | 8.56 | 41. 42 | 3.15 | 25.8 | 234 |
350 | 0.95 | 13.88 | 55.54 | 7.32 | 7.9 | 738 |
400 | 0.89 | 12.71 | 56.89 | 6.43 | 12.5 | 698 |