Fig. 1From: Preparation of NASICON-Type Nanosized Solid Electrolyte Li1.4Al0.4Ti1.6(PO4)3 by Evaporation-Induced Self-Assembly for Lithium-Ion BatteryTGA curve of the dried gel for LATP precursors prepared by EISA method (heating rate 10 °C min−1, air atmosphere)Back to article page