Fig. 1From: Smooth ZnO:Al-AgNWs Composite Electrode for Flexible Organic Light-Emitting DeviceThe flow-process of fabricating flexible electrode. a Dropping AgNWs solution and spin coating. b Drying in the oven at 150 °C. c Patterning electrode. d Dropping NOA63 and spin coating. e Exposing under ultraviolet light with 300–370 nm wavelength for 4 min. f Peeling the NOA63 off. g Depositing AZO by ALDBack to article page