Table 1 The comparison of discharge capacities for different samples
From: Tin Oxide-Carbon-Coated Sepiolite Nanofibers with Enhanced Lithium-Ion Storage Property
Sample | 1st | 2nd | 10th | 20th | 50th | 100th |
---|---|---|---|---|---|---|
Reported SnO2 [17] | 1600.3 | 1100.1 | 646.9 | 485.9 | 145.1 | – |
Experimental SnO2 | 1383.9 | 741.6 | 507.3 | 448.5 | 353.1 | 213.0 |
Experimental SnO2 –C@Sep | 1271.6 | 500.4 | 381.0 | 325.1 | 271.9 | 219.3 |