Skip to main content
Account

Table 4 Sorption capacity towards U(VI) and regeneration of the samples

From: Formation of Zirconium Hydrophosphate Nanoparticles and Their Effect on Sorption of Uranyl Cations

Sample

A  × 104, mol g−1

Regeneration degree, %

C i  = 1 × 10−5 M

C i  = 1 × 10−3 M

Water

Na2SO4

H2SO4

Total

Pristine resin

0.042

4.00

2

60

38

100

CR-3

0.099

3.95

2

15

83

100

CR-7

0.098

5.07

2

24

74

100