Fig. 2From: Effect of Severe Plastic Deformation on Structure and Properties of Al-Sc-Ta and Al-Sc-Ti AlloysThe structure of Al-0.6%Sc-0.05%Ta alloy after deformation: HE, e = 0.74, cross-section (a); longitudinal section (b); 1ECAH + HE, e Σ = 1.9, cross-section (c); longitudinal section (d)Back to article page