Fig. 4From: Effect of Severe Plastic Deformation on Structure and Properties of Al-Sc-Ta and Al-Sc-Ti AlloysChanges in the deformation structure of the Al-0.3%Sc alloy after annealing: the initial deformation HE + 5ECAH + HE, e Σ = 6.8 (a); the deformation e Σ = 6.8 + isochronal annealing at 300 °C (τ = 2 h) + 400 °C (τ = 2 h) + 450 °C (τ = 2 h) (b)Back to article page