Fig. 9From: Effect of Severe Plastic Deformation on Structure and Properties of Al-Sc-Ta and Al-Sc-Ti AlloysThe microstructure of the alloy after SPD e Σ = 6.8 + aging: Al-0.3%Sc, aging at 350 °C for 2 h (a); Al-0.3%Sc, aging at 450 °C for 2 h (b); Al-0.6%Sc-0.2%Ta, aging at 450 °C for 2 h (c); Al-0.6%Sc-0.6%Ta, aging 450 °C for 2 h (d); Al-0.3%Sc, aging at 450 °C for 2 h (e); and Al-0.6%Sc-0.6%Ta, aging at 450 °C for 2 h (f)Back to article page