Fig. 5From: Epitaxial Growth of SrTiO3 Films on Cube-Textured Cu-Clad Substrates by PLD at Low Temperature Under Reducing AtmosphereEBSD maps and the corresponding (111) pole figure of STO films grown at a chamber pressure, laser frequency, and substrate temperature of 10−4 mbar, 10 Hz, and 500 °C, respectively, with a thickness of a 500 nm, b 800 nm, c 1000 nm, and d color key for crystal orientation mapBack to article page