From: Optical Constants and Band Gap Evolution with Phase Transition in Sub-20-nm-Thick TiO2 Films Prepared by ALD
ALD cycles
50
100
200
300
400
500
600
Thickness (nm)
2.55
3.45
6.05
9.72
13.90
16.97
20.61