Table 2 Number fraction of atoms with different local crystalline orders in the products sintered under different heating rates
From: Vibration-Induced Property Change in the Melting and Solidifying Process of Metallic Nanoparticles
Heating rate (K/ps) | 0.04 | 0.1 | 0.2 | 0.5 | 1.0 |
---|---|---|---|---|---|
Disordered (%) | 27.5 | 27.5 | 35.6 | 39.8 | 44.8 |
FCC (%) | 32.5 | 45.6 | 40.1 | 37.0 | 30.2 |
HCP (%) | 40.0 | 26.8 | 23.7 | 20.3 | 22.6 |
BCC (%) | 0.0 | 0.1 | 0.6 | 2.9 | 2.4 |