Skip to main content

Advertisement

Table 3 Number fraction of atoms with different local crystalline orders in the products sintered under different vibration amplitudes

From: Vibration-Induced Property Change in the Melting and Solidifying Process of Metallic Nanoparticles

Amplitude 3a 5a 7a
Disordered (%) 27.3 38.1 47.1
FCC (%) 54.9 34.0 32.6
HCP (%) 17.7 26.7 19.0
BCC (%) 0.1 1.2 1.3