Fig. 2From: Interfacial Spin Glass State and Exchange Bias in the Epitaxial La0.7Sr0.3MnO3/LaNiO3 Bilayer a Magnetic hysteresis loops of the four different samples at 5 K after zero field-cooling from room temperature. b The H C and M S of LSMO/LNO bilayer dependence on the LNO layer having different thickness. The M S was obtained after saturating at 2 kOeBack to article page