Table 3 The EDS results of aluminum nanorods precursors doped with different ions
From: Preparation of Alumina Nanorods from Chromium-Containing Alumina Sludge
The samples | Al (At%) | Cr (At%) | Fe (At%) | Mg (At%) | Total (At%) |
---|---|---|---|---|---|
Cr-doped alumina nanorods | 97.94 | 2.06 | – | – | 100.00 |
Fe-doped alumina nanorods | 99.01 | – | 0.99 | – | 100.00 |
Mg-doped alumina nanorods | 99.42 | – | – | 0.58 | 100.00 |
The alumina nanorods prepared from chromium-containing alumina sludge | 96.79 | 2.11 | 0.14 | 0.96 | 100.00 |