Table 2 Comparison of normalized rate (κ nor) of different catalysts for the reduction of 4-NP (at room temperature)
Catalyst | κ app (min−1) | κ nor (min−1g−1L) | Ref. | Issue |
---|---|---|---|---|
Au/TiO2 | 0.17 | 0.34 | [47] | J Catal |
Core-shell Ag@Pt | 0.15 | 0.92 | [48] | J Catal |
Ag/KCC-1 | 0.6 | 9 | [49] | J Catal |
Au/PMMA | 0.43 | 3.25 | [50] | J Mol Catal A-Chem |
meso-Co3O4 | ~0.018 | 0.23 | [51] | Appl. Catal. B: Environ |
Co@SiO2 | 0.82 | 4.08 | [52] | Inorg. Chem. |
rGO/Fe3O4/Au | 0.69 | 0.52 | [53] | Phys. Chem. Chem. Phys |
AgNPs/GR-G3.0PAMAM | 1.30 | 0.78 | [54] | J Mol Catal A-Chem |
Ag | 0.3 | 1.30 | [55] | J. Phys. Chem. C |
Ag | 0.20 | 0.29 | [56] | Catal Sci Technol |
Ag | 0.13 | 0.007 | [57] | J Alloy Compd |
SnO2 | 0.05 | 0.04 | [58] | Mater. Lett. |
SnO2/Ag (36 h)—1st | 3.10 | 6.20 | This work | – |
SnO2/Ag (36 h)—5th | 0.32 | 0.64 | This work | – |
SnO2/Ag (36 h)—10th | 0.28 | 0.54 | This work | – |
Pure SnO2 | 1.24 | 2.48 | This work | – |
Pure Ag | 1.16 | 2.32 | This work | – |