Fig. 4From: Miniaturized Stretchable and High-Rate Linear Supercapacitors a CV curves of bare CNT and PANI@Au x @CNT electrode materials at a scan rate of 100 mV s−1; b CV curves of PANI@Au15@CNT at a scan rate of 1–100 V s−1; c CV curves of supercapacitors based on the bare CNT and PANI@Au15@CNT at a scan rate of 200 mV s−1; d GCD curves of supercapacitors based on the bare CNT and PANI@Au15@CNT electrodes at a current density of 1 A g−1. The CV curves obtained from different scan rates are normalized to 1 V s−1 in b Back to article page