Fig. 5From: Hydrothermal-Assisted Sintering Strategy Towards Porous- and Hollow-Structured LiNb3O8 Anode MaterialThe initial three CV curves of the LiNb3O8 powder at a scan rate of 0.05 mV/s between the voltage ranges of 3–1 VBack to article page