Table 2 Mechanical properties of PVA nanofiber membranes without and with SDBS
From: High-Throughput Fabrication of Quality Nanofibers Using a Modified Free Surface Electrospinning
SDBS (wt%) | Thickness (mm) | Tensile strength (MPa) | Elongation (%) |
---|---|---|---|
0 | 0.11 ± 0.01 | 7.58 | 6.44 |
0.3 | 0.10 ± 0.02 | 9.58 | 95.43 |