Table 3 The evaluation of irradiation hardening of V-4Cr-4Ti alloy that underwent the post-irradiation annealing treatment for 10, 20, and 30 h at 450 °C
Holding time (h) | Dislocation loop | Bubble |
---|---|---|
10 | 4.6A | 54.7B |
20 | 3.7A | 83.7B |
30 | × | 96.2B |
Holding time (h) | Dislocation loop | Bubble |
---|---|---|
10 | 4.6A | 54.7B |
20 | 3.7A | 83.7B |
30 | × | 96.2B |