Fig. 4From: Temperature and Pressure Dependences of the Elastic Properties of Tantalum Single Crystals Under <100> Tensile Loading: A Molecular Dynamics StudyStress-strain curves of 3.96 nm Ta model at the strain rate of 5 × 108 s− 1 and different temperatures from 1 to 1500 K. It can be seen from Fig. 4 that the slopes of these curves that denotes the elastic modulus in <100> orientation, i.e., E100, during elastic tension period and the yielding stress are gradually decreasing with the increasing temperatureBack to article page