Fig. 4From: Preparation and Antibiofilm Properties of Zinc Oxide/Porous Anodic Alumina Composite FilmsSEM images of the porous anodic alumina (PAA) with different times of second anodization duration a 0 min, b 40 min, c 60 min, and d 80 minBack to article page