Table 2 BET specific surface areas of pure Co3O4 nanoparticles and Co3O4/ZnO heterostructures

From: Effect of Zinc Acetate Concentration on Optimization of Photocatalytic Activity of p-Co3O4/n-ZnO Heterostructures

Sample

Co3O4

Co3O4/ZnO-5

Co3O4/ZnO-15

Co3O4/ZnO-25

Co3O4/ZnO-35

Co3O4/ZnO-45

Co3O4/ZnO-55

SBET/m2·g−1

23.97

38.51

40.14

43.48

60.23

26.63

24.19