Skip to main content
Account

Table 3 First-order rate constants of pure Co3O4 nanoparticles and Co3O4/ZnO heterostructures

From: Effect of Zinc Acetate Concentration on Optimization of Photocatalytic Activity of p-Co3O4/n-ZnO Heterostructures

Sample

methyl orange

Co3O4

Co3O4/ZnO-5

Co3O4/ZnO-15

Co3O4/ZnO-25

Co3O4/ZnO-35

Co3O4/ZnO-45

Co3O4/ZnO-55

K (h−1)

0.00157

0.00245

0.01004

0.01697

0.01999

0.03054

0.02248

0.01432