Fig. 7From: Solution Processed Trilayer Structure for High-Performance Perovskite Photodetectora Visible absorption spectra. b XRD spectra. c I–V curves of the trilayer photodetector as made and after 30 days in ambient environment (under the white light intensity of 0.5 mW cm−2)Back to article page