Fig. 1From: Low-Temperature Plasma-Enhanced Atomic Layer Deposition of SiO2 Using Carbon DioxideGPC of PEALD SiO2 films grown on Si substrates as a function of BTBAS a pulse time and b purge time. The applied plasma power was 180 WBack to article page