Fig. 3From: Structural Characterizations and Dielectric Properties of Sphere- and Rod-Like PbTiO3 Powders Synthesized via Molten Salt SynthesisXRD patterns of the TiO2 templates annealed at (a) 600 °C, (b) 700 °C, and (c) 800 °C for 1 hBack to article page