Fig. 6From: The sintering temperature effect on electrochemical properties of Ce0.8Sm0.05Ca0.15O2-δ (SCDC)-La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) heterostructure pelletThe Arrhenius plots of pellet sintered at 600 °C compared to that of pellet obtained at 1000 °C in a total conductivity and b grain boundary conductivityBack to article page