Fig. 1From: ZnO Porous Nanosheets with Partial Surface Modification for Enhanced Charges Separation and High Photocatalytic Activity Under Solar IrradiationXRD patterns of ZnO, BiVO4, and BiVO4-modifying ZnO with different Bi/Zn molar ratios. The enlarged diffraction peaks at 31.8° of ZnO (100) for ZnO, ZB_0.005, and ZB_0.01, and the amplified diffraction peaks at 28.6° of BZVO solution for ZB_0.05, ZB_0.1, and ZB_0.2 are separately shown in a and b on the right, respectivelyBack to article page