Skip to main content
Account

Table 3 Degradation temperature of PBAT, NCs-PBAT/Cu, NCs-PBAT/Cu|Cu2O, and MCs-PBAT/CuSO4

From: Comparative Study of the Antimicrobial Effect of Nanocomposites and Composite Based on Poly(butylene adipate-co-terephthalate) Using Cu and Cu/Cu2O Nanoparticles and CuSO4

Sample

Initial degradation temperature Tdi [°C]

Final degradation temperature Tdf [°C]

% of degradation

PBAT

316.21

420.77

98.92

NCs-PBAT/Cu 1%

337.63

425.83

97.58

NCs-PBAT/Cu 3%

341.38

427.17

95.48

NCs-PBAT/Cu 5%

342.72

427.17

96.80

NCs-PBAT/Cu|Cu2O 1%

352.36

403.6

92.94

NCs-PBAT/Cu|Cu2O 3%

353.24

402.27

92.66

NCs-PBAT/Cu|Cu2O 5%

338.12

403.15

90.25

MCs-PBAT/CuSO4 1%

360.91

401.65

94.12

MCs-PBAT/CuSO4 3%

352.73

401.33

92.12

MCs-PBAT/CuSO4 5%

351.52

396.14

94.71