Table. 1 Analysis data according to TGA curves of Ag NP suspension of S1

From: Nano-Silver Ink of High Conductivity and Low Sintering Temperature for Paper Electronics

Washing times

Weight loss for PVP (300 to 500 °C) (%)

Residual mass of silver (600 °C) (%)

PVP-to-Ag weight ratio

2 times

5.07

92.06

0.0551

3 times

4.81

93.41

0.0515

4 times

4.60

93.92

0.0490

5 times

4.56

93.71

0.0487