Table 2 Analysis data according to TGA curves of different sizes of Ag NP suspension (S1 to S4)

From: Nano-Silver Ink of High Conductivity and Low Sintering Temperature for Paper Electronics

Sample

Size (nm)

Weight loss for PVP (300 to 500 °C) (%)

Residual mass of silver (600 °C) (%)

PVP-to-Ag weight ratio

S1

48 ± 12

5.04

92.92

0.0542

S2

76 ± 33

4.26

94.40

0.0451

S3

158 ± 65

2.64

96.04

0.0275

S4

176 ± 85

1.74

96.90

0.0180