Table 1 Specific surface area (SBET), pore size (Dp) and pore volume (Vp) of the dealloyed Al91.3Ce8Pd0.7 ribbons calcined at different temperatures

From: Rod-Like Nanoporous CeO2 Modified by PdO Nanoparticles for CO Oxidation and Methane Combustion with High Catalytic Activity and Water Resistance

Calcination temperature (°C)

SBET (m2 g−1)

Dp (nm)

Vp (cm3 g−1)

Dealloyed ribbons

80

13.66

0.267

Calcined at 300 °C

101

12.02

0.336

Calcined at 400 °C

102

13.72

0.362

Calcined at 500 °C

85

12.73

0.304

Calcined at 600 °C

84

13.21

0.317