Fig. 20 | Nanoscale Research Letters

Fig. 20

From: Carbon Nanotube Assembly and Integration for Applications

Fig. 20

a SEM image of a two-terminal SWCNT intramolecular junction formed by varying the temperature during CVD growth from 950 to 900 °C (temperatures are indicated by T1 and T2). Adapted from [141]. b The corresponding shift in the Raman spectra with variations in the temperature. Inset shows the schematic illustrations of SWNT diameter variations with temperature. Adapted from [141]