Table 2 The fitting parameters and PL lifetimes

From: Controlled Synthesis and Properties of 3d–4f Metals Co-doped Polyoxometalates-Based Materials

Sample

τ1 (ns)

τ2 (ns)

A1

A2

τav (µs)

CeCdW12

1195.63

8692.14

0.189

0.891

8.48

EuCrMo6

5.94

187.43

1535.43

159.01

1.14