Table 1 The surface area and pore size of the four kinds of ZnO nanostrucutres
From: Anion-Regulated Synthesis of ZnO 1D Necklace-Like Nanostructures with High Photocatalytic Activity
Sample | Zinc precursor | Surface area (m2 g−1) | Pore size (m3 g−1) |
---|---|---|---|
ZnO 1D NNS | Zinc acetate | 60.3 | 0.156 |
ZnO nanoflowers | Zinc nitrate | 33.5 | 0.106 |
ZnO nanoflakes | Zinc chloride | 22.9 | 0.064 |
ZnO nanoplates | Zinc sulfate | 15.8 | 0.036 |