Table 1 Lifetime and enhancement factor of the R6G/glass, R6G/Au NPs/glass and R6G/PMMA/Au NPs/glass samples

From: Distance-Dependent Plasmon-Enhanced Fluorescence of Submonolayer Rhodamine 6G by Gold Nanoparticles

Sample

Density of PMMA (wt%)

Enhancement factor

τ1 (ns), A1

τ2 (ns), A2

τ3 (ns), A3

R6G/Au NPs/glass

3.78

0.42, 4

2.66, 67

5.68, 29

R6G/PMMA/Au NPs/glass

0.03

2.6

2.43, 11

5.26, 34

22.89,55

0.1

2.01

0.62, 5

4.89, 30

22.39, 65

0.4

1.67

0.55, 10

3.07, 62

13.09, 28

R6G/glass

1