Fig. 8From: MoS2 with Controlled Thickness for Electrocatalytic Hydrogen EvolutionCV curves of a 50ALD-MoS2/GC, b 100ALD-MoS2/GC, c 150ALD-MoS2/GC, d 200ALD-MoS2/GC, and e 250ALD-MoS2/GC measured in 0.5 M H2SO4 in the non-Faradaic region with different scan rates from 20 to 140 mV s−1. f Differences of anodic and cathodic current densities at 0.15 V versus RHE as the functions of scan rateBack to article page