Fig. 2
From: Transfer Printing of Perovskite Whispering Gallery Mode Laser Cavities by Thermal Release Tape

Microscopic images of perovskite nanoplatelets adhere to thermal release tape after pressing nanoplatelets/tape with 0.45 MPa (a), 0.50 MPa (b), 0.55 MPa (c) pressure for 3 min and 0.50 MPa pressure for 2 min (d), 3 min (e) and 4 min (f) before mechanical exfoliation