Table 3 Contact angle, θ, measured for as-prepared and treated ZnO nanomaterial

From: Wettability Modification of Nanomaterials by Low-Energy Electron Flux

 

1-Bromonaphtalene

Ethylene glycol

Diiodomethane

Formamide

Water

As-prepared ZnO nanomaterial

9 ± 1

63 ± 1

66 ± 2

52 ± 3

60 ± 4

UV illuminated

8 ± 2

14 ± 2

64 ± 1

20 ± 3

3 ± 1

E-beam irradiated

8 ± 1

72 ± 1

70 ± 2

73 ± 3

85 ± 2